In the creep test, the following type of stress is applied to the specimen
  • a)
    uniaxial compression
  • b)
    uniaxial tension
  • c)
    biaxial compression or tension
  • d)
    alternating stress
Correct answer is option 'B'. Can you explain this answer?
Verified Answer
In the creep test, the following type of stress is applied to the spec...
In the creep test, uniaxial tension is applied to the specimen. The purpose of the test is to measure the deformation of a material under a sustained load, which is often known as creep deformation, over a certain period of time. The test is typically used to evaluate the behavior of a material when subjected to long-term loads and it can provide information on the strength and ductility of the material, as well as its ability to maintain its properties under sustained loads. The test requires a specialized testing machine, which can apply a constant load to the specimen while monitoring the deformation over time. The results are typically presented in the form of a creep curve, which plots the deformation of the specimen over time.
View all questions of this test
Most Upvoted Answer
In the creep test, the following type of stress is applied to the spec...
**Explanation:**

The creep test is a type of mechanical test used to determine the behavior of a material under a constant load over an extended period of time. It is used to study the phenomenon of creep, which is the time-dependent deformation of a material under a constant stress.

The type of stress applied to the specimen in the creep test is uniaxial tension. This means that the specimen is subjected to a constant tensile load in one direction, while the other dimensions of the specimen are constrained.

**Reasons for the Correct Answer:**

- Uniaxial tension is the most common type of stress applied in the creep test because it allows for a controlled and consistent loading condition.
- The applied tensile stress causes the material to elongate over time, and the amount of elongation is measured at specified time intervals.
- This allows for the determination of the creep behavior of the material, including the creep rate and the steady-state creep rate.
- Uniaxial tension is chosen over other types of stress, such as compression or alternating stress, because it is easier to apply and measure in a laboratory setting.
- Biaxial compression or tension involves applying stress in more than one direction, which adds complexity to the test setup and analysis.
- Alternating stress involves cyclic loading and unloading, which is not suitable for studying the time-dependent deformation of a material.

**Conclusion:**

In the creep test, the type of stress applied to the specimen is uniaxial tension. This allows for the controlled measurement of the time-dependent deformation of the material under a constant tensile load. The use of uniaxial tension simplifies the test setup and analysis, making it a common and practical choice for studying creep behavior.
Explore Courses for Civil Engineering (CE) exam

Top Courses for Civil Engineering (CE)

Question Description
In the creep test, the following type of stress is applied to the specimena)uniaxial compressionb)uniaxial tensionc)biaxial compression or tensiond)alternating stressCorrect answer is option 'B'. Can you explain this answer? for Civil Engineering (CE) 2025 is part of Civil Engineering (CE) preparation. The Question and answers have been prepared according to the Civil Engineering (CE) exam syllabus. Information about In the creep test, the following type of stress is applied to the specimena)uniaxial compressionb)uniaxial tensionc)biaxial compression or tensiond)alternating stressCorrect answer is option 'B'. Can you explain this answer? covers all topics & solutions for Civil Engineering (CE) 2025 Exam. Find important definitions, questions, meanings, examples, exercises and tests below for In the creep test, the following type of stress is applied to the specimena)uniaxial compressionb)uniaxial tensionc)biaxial compression or tensiond)alternating stressCorrect answer is option 'B'. Can you explain this answer?.
Solutions for In the creep test, the following type of stress is applied to the specimena)uniaxial compressionb)uniaxial tensionc)biaxial compression or tensiond)alternating stressCorrect answer is option 'B'. Can you explain this answer? in English & in Hindi are available as part of our courses for Civil Engineering (CE). Download more important topics, notes, lectures and mock test series for Civil Engineering (CE) Exam by signing up for free.
Here you can find the meaning of In the creep test, the following type of stress is applied to the specimena)uniaxial compressionb)uniaxial tensionc)biaxial compression or tensiond)alternating stressCorrect answer is option 'B'. Can you explain this answer? defined & explained in the simplest way possible. Besides giving the explanation of In the creep test, the following type of stress is applied to the specimena)uniaxial compressionb)uniaxial tensionc)biaxial compression or tensiond)alternating stressCorrect answer is option 'B'. Can you explain this answer?, a detailed solution for In the creep test, the following type of stress is applied to the specimena)uniaxial compressionb)uniaxial tensionc)biaxial compression or tensiond)alternating stressCorrect answer is option 'B'. Can you explain this answer? has been provided alongside types of In the creep test, the following type of stress is applied to the specimena)uniaxial compressionb)uniaxial tensionc)biaxial compression or tensiond)alternating stressCorrect answer is option 'B'. Can you explain this answer? theory, EduRev gives you an ample number of questions to practice In the creep test, the following type of stress is applied to the specimena)uniaxial compressionb)uniaxial tensionc)biaxial compression or tensiond)alternating stressCorrect answer is option 'B'. Can you explain this answer? tests, examples and also practice Civil Engineering (CE) tests.
Explore Courses for Civil Engineering (CE) exam

Top Courses for Civil Engineering (CE)

Explore Courses
Signup for Free!
Signup to see your scores go up within 7 days! Learn & Practice with 1000+ FREE Notes, Videos & Tests.
10M+ students study on EduRev