Silicon content in iron lamination is kept within 5% as it-
  • a)
    makes the material brittle
  • b)
    reduces the curie point
  • c)
    increased hysteresis loss
  • d)
    increased cost
Correct answer is option 'A'. Can you explain this answer?
Verified Answer
Silicon content in iron lamination is kept within 5% as it-a)makes th...
Silicon content in Iron lamination is kept within 5% as it makes the material brittle.
View all questions of this test
Most Upvoted Answer
Silicon content in iron lamination is kept within 5% as it-a)makes th...
Explanation:

Silicon content in iron lamination is kept within 5% as it makes the material brittle. This is because of the following reasons:

1. Effect on Ductility: Ductility is the ability of a material to undergo plastic deformation without fracture. When the silicon content in iron lamination increases beyond 5%, it reduces the ductility of the material. This means that the material becomes more brittle and prone to cracking under stress.

2. Effect on Hardness: The increase in silicon content also increases the hardness of the material. This means that the material becomes more resistant to deformation and less malleable. This can make it difficult to shape the material into the desired form.

3. Effect on Magnetic Properties: The magnetic properties of iron lamination are important for its use in electrical equipment. The increase in silicon content can reduce the magnetic permeability of the material, which can result in increased hysteresis loss and reduced efficiency.

Conclusion:

In conclusion, the silicon content in iron lamination is kept within 5% to ensure that the material remains ductile and malleable. This helps to prevent cracking and makes it easier to shape the material. Additionally, keeping the silicon content low helps to maintain the magnetic properties of the material, which is important for its use in electrical equipment.
Explore Courses for SSC exam
Silicon content in iron lamination is kept within 5% as it-a)makes the material brittleb)reduces the curie pointc)increased hysteresis lossd)increased costCorrect answer is option 'A'. Can you explain this answer?
Question Description
Silicon content in iron lamination is kept within 5% as it-a)makes the material brittleb)reduces the curie pointc)increased hysteresis lossd)increased costCorrect answer is option 'A'. Can you explain this answer? for SSC 2024 is part of SSC preparation. The Question and answers have been prepared according to the SSC exam syllabus. Information about Silicon content in iron lamination is kept within 5% as it-a)makes the material brittleb)reduces the curie pointc)increased hysteresis lossd)increased costCorrect answer is option 'A'. Can you explain this answer? covers all topics & solutions for SSC 2024 Exam. Find important definitions, questions, meanings, examples, exercises and tests below for Silicon content in iron lamination is kept within 5% as it-a)makes the material brittleb)reduces the curie pointc)increased hysteresis lossd)increased costCorrect answer is option 'A'. Can you explain this answer?.
Solutions for Silicon content in iron lamination is kept within 5% as it-a)makes the material brittleb)reduces the curie pointc)increased hysteresis lossd)increased costCorrect answer is option 'A'. Can you explain this answer? in English & in Hindi are available as part of our courses for SSC. Download more important topics, notes, lectures and mock test series for SSC Exam by signing up for free.
Here you can find the meaning of Silicon content in iron lamination is kept within 5% as it-a)makes the material brittleb)reduces the curie pointc)increased hysteresis lossd)increased costCorrect answer is option 'A'. Can you explain this answer? defined & explained in the simplest way possible. Besides giving the explanation of Silicon content in iron lamination is kept within 5% as it-a)makes the material brittleb)reduces the curie pointc)increased hysteresis lossd)increased costCorrect answer is option 'A'. Can you explain this answer?, a detailed solution for Silicon content in iron lamination is kept within 5% as it-a)makes the material brittleb)reduces the curie pointc)increased hysteresis lossd)increased costCorrect answer is option 'A'. Can you explain this answer? has been provided alongside types of Silicon content in iron lamination is kept within 5% as it-a)makes the material brittleb)reduces the curie pointc)increased hysteresis lossd)increased costCorrect answer is option 'A'. Can you explain this answer? theory, EduRev gives you an ample number of questions to practice Silicon content in iron lamination is kept within 5% as it-a)makes the material brittleb)reduces the curie pointc)increased hysteresis lossd)increased costCorrect answer is option 'A'. Can you explain this answer? tests, examples and also practice SSC tests.
Explore Courses for SSC exam
Signup for Free!
Signup to see your scores go up within 7 days! Learn & Practice with 1000+ FREE Notes, Videos & Tests.
10M+ students study on EduRev